Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ASTM D149 |
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 2215 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ASTM D149 |
IDI Composites 46-16-60 Thermoset Polyester, Sheet TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer. |
|||
Dielectric Strength | 8.70 kV/mm @Thickness 1.59 mm |
221 kV/in @Thickness 0.0625 in |
100% RH for 96 hours; ASTM D149 |
Garlock GYLON® 3565 ENVELON® PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microsphere filler.Soft, deformable exterior conforms to surface irregularities; ideal for worn, warped or pitted flangesStable blue core improves cold flow resistanceLow b.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ac; ASTM D116 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ac; ASTM D116 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ac; ASTM D116 |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | AC; ASTM D116 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | |
Du-Co Ceramics DC-10-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | ASTM D149 |
3D Systems DuraForm® GF Glass Filled Nylon For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o.. |
|||
Dielectric Strength | 8.70 kV/mm | 221 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 2020 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |