Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.80 kV/mm | 224 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Dielectric Strength | 8.80 kV/mm | 224 kV/in | Short Time; ASTM D149 |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Dielectric Strength | 8.80 kV/mm | 224 kV/in | Short Time; ASTM D149 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Dielectric Strength | 8.80 kV/mm | 224 kV/in | Short Time; ASTM D149 |
Plenco 7467 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved .. |