Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.7 kV/mm | 830 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | ASTM D149 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
Dielectric Strength | 32.7 kV/mm | 831 kV/in | ASTM D149 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | In Air; ASTM D149 |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Dielectric Strength | 32.7 kV/mm @Thickness 0.762 mm |
830 kV/in @Thickness 0.0300 in |
ASTM D149 |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | ASTM D149 |
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti.. |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | ASTM D149 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
Dielectric Strength | 32.7 kV/mm | 830 kV/in | ASTM D149 |
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 32.7 kV/mm | 831 kV/in | Arlon-SQA-TMS-020 |
Arlon 44278R018B 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 1: Cured Silicone RubberInterleave: LDPEUL R.. |