Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 315 kV/mm | 8000 kV/in | ASTM D1000 |
3M 9731 Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Dielectric Strength | 315 kV/mm | 8000 kV/in | ASTM D1000 |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |