Polymer Property : Dielectric Strength = 26.1 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 26.1 kV/mm

@Thickness 1.50 mm
663 kV/in

@Thickness 0.0591 in
in oil; IEC 60243-1
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Dielectric Strength 26.1 kV/mm
664 kV/in
ASTM D149
Arlon 51250R016 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data should not be u..