Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.80 kV/mm | 71.1 kV/in | 1" Axial in Oil; ASTM D-149 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Dielectric Strength | 2.80 kV/mm | 71.1 kV/in | IEC 672-1 |
CeramTec SL 303 Silicon Nitride, SiAION+SiC SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i.. |
|||
Dielectric Strength | 2.80 kV/mm | 71.0 kV/in | |
Zircar Refractory Composites RS-100 Refractory Sheet ZIRCAR Refractory Sheet Type RS-100 is a ceramic fiber reinforced structural alumina composite material with useful properties to 1260°C (2300°F). It has exceptional flexural and compressive stren.. |
|||
Dielectric Strength | 2.80 kV/mm | 71.0 kV/in | |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Dielectric Strength | 2.80 kV/mm @Diameter >=3.00 mm |
71.1 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi.. |