Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.6 kV/mm | 395 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet) |
|||
Dielectric Strength | >= 15.6 kV/mm @Temperature 121 °C, Time 10800 sec |
>= 396 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | |
Momentive Performance Materials RTV112 White Adhesive Sealant, General Purpose Pourable One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Thin-section protective .. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | |
Momentive Performance Materials RTV118 Translucent Adhesive Sealant, General Purpose Pourable One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Thin-section protective .. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | |
Momentive Performance Materials RTV159 Red Adhesive Sealant, High Strength Paste One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance.. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | Short Time; ASTM D149 |
Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | Step by Step; ASTM D149 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Dielectric Strength | 15.6 kV/mm | 395 kV/in | |
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation con.. |
|||
Dielectric Strength | 15.6 kV/mm | 395 kV/in | |
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting.. |
|||
Dielectric Strength | 15.6 kV/mm | 395 kV/in | |
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the.. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | Short time, 500 V/sec rate-of-rise; ASTM D149 |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Dielectric Strength | 15.6 - 16.8 kV/mm | 396 - 427 kV/in | ASTM D149-97a |
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi.. |
|||
Dielectric Strength | 15.6 kV/mm | 396 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |