Polymer Property : Dielectric Strength = 15.25 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 350E0096912 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 13%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, ..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate  (discontinued **)
Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Dielectric Strength 15.25 kV/mm
387.4 kV/in
ASTM D149
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..