Polymer Property : Dielectric Strength = 126 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 126 kV/mm

@Thickness 0.0762 mm
3200 kV/in

@Thickness 0.00300 in
ASTM D149
Westlake Plastics PEEK Film Made from VICTREX® Polymer
Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excelle..
Dielectric Strength 126 kV/mm
3200 kV/in
0.25 inch electrodes in dry air @25°C; ASTM D149-81
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..