Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.60 - 59.1 kV/mm | 40.6 - 1500 kV/in | Average value: 21.3 kV/mm Grade Count:455 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Dielectric Strength | 1.60 kV/mm | 40.6 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Dielectric Strength | 1.60 kV/mm @Diameter >=3.00 mm |
40.6 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac.. |