Polymer Property : Curie Temperature = -110 °F
Polymer Property :
Curie Temperature =
-110 °F
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Curie Temperature
<=
-79.0
°C
<=
-110
°F
Annealed and Furnace-cooled
Special Metals MONEL® 404 Copper-Nickel Alloy
Data provided by California Fine Wire and the manufacturer, Special Metals.