Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 10000 Gauss | 10000 Gauss | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 1 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Magnetic Remanence, Br | 10000 Gauss | 10000 Gauss | |
Alliance A-6S Alnico Magnetic Material |
|||
Magnetic Remanence, Br | 10000 Gauss | 10000 Gauss | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |