Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 8100 - 8500 Oe | 8100 - 8500 Oe | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |