Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | >= 5.00e+6 ohm @Diameter 8.00 - 10.0 mm |
>= 5.00e+6 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+6 ohm @Diameter 8.00 - 10.0 mm |
>= 5.00e+6 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CC 41 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Fine weave (more than 30 threads per cm).Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+6 ohm @Diameter 8.00 - 10.0 mm |
>= 5.00e+6 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe. |
|||
Insulation Resistance | 5.00e+6 ohm @Thickness >=3.00 mm |
5.00e+6 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Insulation Resistance | 5.00e+6 ohm @Thickness >=3.00 mm |
5.00e+6 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr.. |
|||
Insulation Resistance | 5.00e+6 ohm @Thickness >=3.00 mm |
5.00e+6 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha.. |