Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Insulation Resistance | 1000 - 100000 ohm | 1000 - 100000 ohm | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | 1000 - 100000 ohm | 1000 - 100000 ohm | |
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L.. |
|||
Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG.. |
|||
Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info.. |