Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 648 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 553 PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 701 PBT (Asia Pacific)
35% glass/mineral alloy, excellent electrical performance to dielectric breakdown. Developed for automotive distributor caps.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Dielectric Strength 25.5 kV/mm

@Thickness 1.60 mm
648 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
Copyright © lookpolymers.com All Rights Reserved