Electrical Properties Metric English Comments
Dielectric Strength 4.00 kV/mm

@Thickness 3.00 mm
102 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Dielectric Strength 4.00 kV/mm

@Thickness 3.00 mm
102 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets