Electrical Properties Metric English Comments
Dielectric Strength 2.40 kV/mm

@Temperature 121 °C,
Time 10800 sec
61.0 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
Garlock GYLON® 3540 Microcellular PTFE Gasketing
Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronit I Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity.Application: Insulation material in hig..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Dielectric Strength 2.40 kV/mm

@Thickness >=3.00 mm
61.0 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Copyright © lookpolymers.com All Rights Reserved