Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.3 kV/mm @Frequency 60.0 Hz |
389 kV/in @Frequency 60.0 Hz |
short time, wet; ASTM D149 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |