Dielectric Strength >= 14.8 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 375 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
Garlock 2920 Compressed Aramid Fiber Gasketing, SBR Binder
Aramid fibers with a SBR binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, steam, inert gases, mild acids and mild alkaliesInform..
Dielectric Strength 14.8 kV/mm

@Thickness 1.57 mm
375 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Dielectric Strength 14.8 kV/mm

@Frequency 60.0 Hz
376 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy
E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Dielectric Strength 14.8 kV/mm

@Frequency 60.0 Hz
376 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy
E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Copyright © lookpolymers.com All Rights Reserved