Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 14.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 14.3 kV/mm

@Frequency 60.0 Hz
363 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir..
Copyright © lookpolymers.com All Rights Reserved