Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 46 - 55 dB @Frequency 1.00e+8 Hz |
46 - 55 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX DS0036I PC LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East) LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex DS0036IC PC (Europe-Africa-Middle East) LNP* FARADEX* DS0036IC is a compound based on Polycarbonate resin, containing Stainless Steel Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, High I.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex DS0036IP PC LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific) LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East) LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East) LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated F.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX MS002 PP LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Shielding Effectiveness | 40 - 55 dB @Thickness 3.00 mm |
40 - 55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |