Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 80 - 100 dB | 80 - 100 dB | modified specimen 0.85 mm x 1.0 mm bead with plastic bolts; MIL-G-83528 Para. 4.6.12 |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+10 Hz |
>= 80 dB @Frequency 1.00e+10 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 80 dB | >= 80 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 2.00e+9 Hz |
>= 80 dB @Frequency 2.00e+9 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+9 Hz |
>= 80 dB @Frequency 1.00e+9 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |