Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | <= 0.50 sec @Thickness 2.00 mm |
<= 0.50 sec @Thickness 0.0787 in |
sheet; IEC 61340-5-1 |
Panipol Oy DXH Inherently Conductive Polymer Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade.. |
|||
Static Decay | <= 0.50 sec | <= 0.50 sec | 5kV to 50V; FTMS 101C |
Kostat BK-STAT 7048BK ABS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Static Decay | <= 0.50 sec | <= 0.50 sec | 5kV to 50V; FTMS 101C |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Static Decay | <= 0.50 sec | <= 0.50 sec | 5kV to 50V; FTMS 101C |
Kostat BK-STAT P048BK PP Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |