Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 1.03 sec Grade Count:7 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 0.543 sec Grade Count:5 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 0.396 sec Grade Count:5 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Static Decay | 0.0100 - 0.100 sec | 0.0100 - 0.100 sec | Average value: 0.0400 sec Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 1.00 sec Grade Count:8 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 0.862 sec Grade Count:17 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 0.921 sec Grade Count:12 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 1.04 sec Grade Count:48 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec | Average value: 1.00 sec Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |