Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 120 - 150 sec | 120 - 150 sec | Average value: 136 sec Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |