Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 77.0 - 146 sec | 77.0 - 146 sec | Average value: 121 sec Grade Count:3 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Arc Resistance | 77.0 - 129 sec | 77.0 - 129 sec | Average value: 109 sec Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |