Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 175 sec | 175 sec | at 500 Volts; ASTM D495 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Arc Resistance | 175 sec | 175 sec | ASTM D495 |
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Arc Resistance | 175 sec | 175 sec | ASTM D495 |
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit.. |
|||
Arc Resistance | 175 sec | 175 sec | ASTM D495 |
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Arc Resistance | 175 sec | 175 sec | ASTM D495 |
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI.. |