Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 131 sec | 131 sec | UL recognition value, tungsten electrode; ASTM D495 |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Arc Resistance | 131 sec | 131 sec | ASTM D495 |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Arc Resistance | 131 sec | 131 sec | ASTM D495 |
Plenco 3557 Phenolic, Granular, Transfer Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |