Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Arc Resistance | 186 sec | 186 sec | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Arc Resistance | >= 186 sec | >= 186 sec | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Arc Resistance | >= 186 sec | >= 186 sec | |
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic.. |
|||
Arc Resistance | >= 186 sec | >= 186 sec | |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Arc Resistance | 186 sec | 186 sec | ASTM D495 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |