Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 3.00e+15 ohm | 3.00e+15 ohm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Surface Resistivity per Square | 3.00e+15 ohm | 3.00e+15 ohm | GB/T1410-2006 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Surface Resistivity per Square | 3.00e+15 ohm | 3.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4116 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |