Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+7 - 1.00e+10 ohm | 1.00e+7 - 1.00e+10 ohm | ASTM D257 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | EOS/ESD S11.11 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |