Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 1e+14 ohm | <= 1e+14 ohm | ASTM D257 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1e+14 ohm | >= 1e+14 ohm | ASTM D257 |
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet) |