Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 42 V | 42 V | IEC 112 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Comparative Tracking Index | 42 V | 42 V | IEC 112 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |