Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 0.000 - 600 V | 0.000 - 600 V | Average value: 339 V Grade Count:34 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Comparative Tracking Index | 0.000 - 400 V | 0.000 - 400 V | Average value: 223 V Grade Count:16 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Comparative Tracking Index | 0.000 - 400 V | 0.000 - 400 V | Average value: 243 V Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Comparative Tracking Index | 0.000 - 250 V | 0.000 - 250 V | Average value: 138 V Grade Count:262 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |