Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 6.37e+9 ohm @Time 605000 sec |
6.37e+9 ohm @Time 168 hour |
Control; IPC B24 |
Indium Corp. WF-9942 Wave Solder Flux, No-Residue WF-9942 Wave Soldering Flux is a no-clean flux specifically developed for wave soldering, mixed-technology and through-hole electronic assemblies. This formulations provides greater heat stability .. |