Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 500 °C |
0.000135 ohm-cm @Temperature 932 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Electrical Resistivity | 0.000135 ohm-cm @Temperature 600 °C |
0.000135 ohm-cm @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |