Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000134 ohm-cm @Temperature 200 °C |
0.000134 ohm-cm @Temperature 392 °F |
|
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 649 °C |
0.000134 ohm-cm @Temperature 1200 °F |
|
ATI Allegheny Ludlum ALFA-II™ Stainless Steel Type 406 Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 800 °C |
0.000134 ohm-cm @Temperature 1470 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 900 °C |
0.000134 ohm-cm @Temperature 1650 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |
|||
Electrical Resistivity | 0.000134 ohm-cm @Temperature 500 °C |
0.000134 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |