Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 20.0 °C |
0.000121 ohm-cm @Temperature 68.0 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Electrical Resistivity | 0.000121 ohm-cm @Temperature 300 °C |
0.000121 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |