Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000986 ohm-cm @Temperature -184 °C |
0.0000986 ohm-cm @Temperature -299 °F |
|
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |