Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+15 - 3.00e+15 ohm | 1.00e+15 - 3.00e+15 ohm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Surface Resistance | 1.00e+13 - 3.00e+15 ohm | 1.00e+13 - 3.00e+15 ohm | Average value: 4.48e+14 ohm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |