Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 9.00e+9 - 4.00e+11 ohm | 9.00e+9 - 4.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Surface Resistance | 9.00e+9 ohm | 9.00e+9 ohm | 12% RH; ESD S11.11 |
Lubrizol Stat-Rite® M-809 Static Control Acrylic Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protec.. |