Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.80e+10 ohm | 4.80e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 1A20 Urethane Conformal Coating Humiseal 1A20 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Surface Resistance | 4.80e+10 ohm | 4.80e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 1A20LSE Urethane Conformal Coating Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther.. |
|||
Surface Resistance | 4.80e+10 ohm | 4.80e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |