Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.10e+14 ohm | 1.10e+14 ohm | ASTM D257 |
Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer Description: Thermoplastic elastomer material with rubber-like flexibility and functionality.DuraForm FlexSeal Infiltration:FlexSeal fluid infiltration is an easy-to-use method of coloring, strength.. |
|||
Surface Resistance | 1.10e+14 ohm | 1.10e+14 ohm | IEC 60093 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Surface Resistance | 1.10e+14 ohm | 1.10e+14 ohm | DAM; IEC 60093 |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Surface Resistance | 1.10e+14 ohm | 1.10e+14 ohm | ASTM D257 |
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems Thermoplastic elastomer material with rubber-like flexibility and functionality. For use with all selective laser sintering SLS® systems.ApplicationsAthletic footwear and equipmentGaskets, hoses an.. |