Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 39.0 - 4.00e+14 ohm | 39.0 - 4.00e+14 ohm | Average value: 8.35e+13 ohm Grade Count:6 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Surface Resistance | 2500 - 4.00e+14 ohm | 2500 - 4.00e+14 ohm | Average value: 2.37e+13 ohm Grade Count:46 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Surface Resistance | 5.00e+11 - 4.00e+14 ohm | 5.00e+11 - 4.00e+14 ohm | Average value: 1.11e+14 ohm Grade Count:4 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |