Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.00e+13 ohm | 7.00e+13 ohm | Condition A; IPC 2.5.17.1 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Surface Resistance | 7.00e+13 ohm | 7.00e+13 ohm | ASTM D257 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Surface Resistance | 7.00e+13 ohm | 7.00e+13 ohm | ASTM D257 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |