Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 60093 |
DSM Akulon® F232-DH Nylon 6 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Surface Resistance | >= 5.00e+14 ohm | >= 5.00e+14 ohm | 500V; Ø 93x3mm; IEC 93 |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 93 |
Solvay Technyl® A 205F Nylon 66, EH0 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 60093 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 60093 |
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon 35N Fast Cure Polyimide Laminate and Prepreg High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi.. |
|||
Surface Resistance | >= 5.00e+14 ohm | >= 5.00e+14 ohm | |
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Surface Resistance | >= 5.00e+14 ohm | >= 5.00e+14 ohm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Surface Resistance | 5.00e+14 ohm | 5.00e+14 ohm | IEC 60093 |
DSM Akulon® K223-TP4 (Cond.) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Surface Resistance | >= 5.00e+14 ohm | >= 5.00e+14 ohm | 500V; Ø 93x3mm; IEC 93 |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |
|||
Surface Resistance | >= 5.00e+14 ohm | >= 5.00e+14 ohm | 500V; Ø 93x3mm; IEC 93 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |