Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.00e+8 ohm | 3.00e+8 ohm | DIN 53482 |
DSM Fibre Intermediates Nyrim® 3000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Surface Resistance | 3.00e+8 ohm | 3.00e+8 ohm | ASTM D257 |
Arkema Group Pebax® MV1074 Polyether Block Amide |
|||
Surface Resistance | 3.00e+8 ohm | 3.00e+8 ohm | |