Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 20.0 - 1.00e+7 ohm | 20.0 - 1.00e+7 ohm | Average value: 1.11e+6 ohm Grade Count:13 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |