Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.030 - 0.045 ohm @Thickness 0.0100 mm |
0.030 - 0.045 ohm @Thickness 0.000394 in |
Printed onto 125µm PET film |
Gwent Electronic Materials C2030922D1 Silver Ink Silver Ink C2030922D1 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass and ceramic to form conductive tracks. The ink should be gently stirred before use avo.. |
|||
Surface Resistivity per Square | 0.030 - 0.045 ohm @Thickness 0.0100 mm |
0.030 - 0.045 ohm @Thickness 0.000394 in |
Printed onto 125 µm PET film |
Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste This product is a screen printable polymer paste designed as a counter electrode in electrochemical biosensors. This ink can be used in conjunction with our working carbon electrode ink C2030519P4, .. |